YG15 stud for cement mine roller crushing
YG15 stud for cement mine roller crushing
YG15 stud for cement mine roller crushing
YG15 stud for cement mine roller crushing

YG15 stud for cement mine roller crushing


As the core parts of the roller press, the hard alloy stud provides high wear resistance and high compressive strength for the roller press, which can meet the requirements of different working conditions. The hard alloy stud used in roller press is suitable for crushing all kinds of rock in metal ore, which can meet the operation requirements such as iron ore and has high working efficiency.

Inquiry
  • Standard

Product Introduction:

As the core parts of the roller press, the hard alloy stud provides high wear resistance and high compressive strength for the roller press, which can meet the requirements of different working conditions. The hard alloy stud used in roller press is suitable for crushing all kinds of rock in metal ore, which can meet the operation requirements such as iron ore and has high working efficiency.


Product Features:

1. The corner adopts arc chamfering transition to avoid local damage in the process of production, transportation, installation and use.

2. Sintering by overpressure sintering, the product has good density and high strength.

3. Using special technology, eliminate the surface stress of the product after processing, and increase the surface hardness.


Product application scope:Mainly used for crushing by roller press


Composite chamfered tungsten steel nail column production characteristics:

1. Spherical crown adopts hemispherical design to avoid stress concentration and damage of steel body

2. The corner adopts arc transition to avoid local damage in the process of production, transportation, installation and use

3. Sintering by pressure sintering, the product has good density and high strength

4. The use of special technology, eliminate the surface stress of the product after processing, and increase the surface hardness

5. Apply a layer of grease on the product surface to avoid oxidation on the product surface


Product brand:

BrandDensity g/cm³Hardness HVRFlexural strength MPaProcessing accuracy
YG613.8g/cm³88.2HVR3100MPa±0.005mm
YG1114.4g/cm³87HVR2500MPa±0.005mm
YG1313.9g/cm³85.5HVR2350MPa±0.005mm
YG1514g/cm³86HVR2800MPa±0.005mm
YG2013.5g/cm³85.5HVR3200MPa±0.005mm